Mechanical Properties Metric English Comments
Tensile Stress 9.86 MPa

@Strain 300 %
1430 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P3991 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 9.86 MPa

@Strain 149.65 %,
Temperature 100 °C
1430 psi

@Strain 149.65 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers
Tensile Stress 9.84 MPa

@Strain 26.77 %,
Temperature 100 °C
1430 psi

@Strain 26.77 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 9.85 MPa

@Strain 144.61 %,
Temperature 90.0 °C
1430 psi

@Strain 144.61 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 9.85 MPa

@Strain 0.150 %,
Temperature 40.0 °C
1430 psi

@Strain 0.150 %,
Temperature 104 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FE350064 BK544 Polyphthalamide (PPA)  (Unverified Data**)
Carbon Fiber Reinforced Toughened PPA High Performance Polyamide Zytel HTNFE350064 BK544 is a carbon fiber reinforced toughened heat stabilized conductive high performance polyamide resin developed ..
Tensile Stress 9.87 MPa

@Strain 0.200 %,
Temperature 150 °C
1430 psi

@Strain 0.200 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FR52G30NH NC010 Polyphthalamide (PPA)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It..
Tensile Stress 9.85 MPa

@Strain 19.43 %,
Temperature 150 °C
1430 psi

@Strain 19.43 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610  (Unverified Data**)
Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by..
Tensile Stress 9.87 MPa

@Strain 171.75 %,
Temperature 150 °C
1430 psi

@Strain 171.75 %,
Temperature 302 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET  (Unverified Data**)
65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers