Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 144.98 MPa @Strain 3.61 %, Temperature 60.0 °C |
21028 psi @Strain 3.61 %, Temperature 140 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® 70G35HSLRA4 BK267 Nylon 66
(Unverified Data**) Zytel® 70G35HSLRA4 BK267 is a 35% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding. It has excellent flow characteristics.Information provided .. |