Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 15.8 MPa @Strain 100 % |
2290 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® EM631 TPC-ET Extrusion Grade |
|||
Tensile Stress | 15.8 MPa @Strain 0.400 %, Temperature 150 °C |
2290 psi @Strain 0.400 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G20NH NC010 Polyphthalamide (PPA)
(Unverified Data**) 20% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G20NH NC010 is a 20% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |
|||
Tensile Stress | 15.8 MPa @Strain 20.0 %, Temperature 23.0 °C |
2290 psi @Strain 20.0 %, Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**) Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac.. |