Mechanical Properties Metric English Comments
Tensile Stress 1.05 MPa

@Strain 100 %
152 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® C4630 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Stress 1.05 MPa

@Strain 100 %
152 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® C4940 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Stress 1.05 MPa

@Strain 100 %,
Temperature 23.0 °C
152 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ CL2242 Thermoplastic Elastomer (TPE)
Versaflex™ CL2242 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov..
Tensile Stress 1.05 MPa

@Strain 100 %
152 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P3650 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 1.05 MPa

@Strain 100 %,
Temperature 23.0 °C
152 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynalloy™ OBC8000-T40 Thermoplastic Elastomer (TPE)
Dynalloy™ OBC8000-T40 is an easy processing, general processing TPE utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. Designed for a wide variety of applications, incl..
Tensile Stress 1.05 MPa

@Strain 25.0 %
152 psi

@Strain 25.0 %
Average; ASTM D412 Method A
Seals Eastern 5722A Fluorocarbon-Elastomer
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Exce..
Tensile Stress 1.05 MPa

@Strain 0.516 %,
Time 3.60e+6 sec
152 psi

@Strain 0.516 %,
Time 1000 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 1.05 MPa

@Strain 0.556 %,
Time 3.60e+7 sec
152 psi

@Strain 0.556 %,
Time 10000 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 1.05 MPa

@Strain 0.444 %,
Time 36000 sec
152 psi

@Strain 0.444 %,
Time 10.0 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 1.05 MPa

@Strain 0.479 %,
Time 360000 sec
152 psi

@Strain 0.479 %,
Time 100 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 1.05 MPa

@Strain 0.412 %,
Time 3600 sec
152 psi

@Strain 0.412 %,
Time 1.00 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 1.05 MPa

@Strain 0.150 %,
Temperature 150 °C
152 psi

@Strain 0.150 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6  (Unverified Data**)
Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers