Polymer Property : Tensile Stress = 1580 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 10.9 MPa

@Strain 100 %
1580 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® VT3104 TPC-ET
Extrusion Grade
Tensile Stress 10.9 MPa

@Strain 60.23 %,
Temperature 90.0 °C
1580 psi

@Strain 60.23 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 10.9 MPa

@Strain 7.67 %,
Temperature 23.0 °C
1580 psi

@Strain 7.67 %,
Temperature 73.4 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET
55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers