Mechanical Properties Metric English Comments
Tensile Stress 11.24 MPa

@Strain 0.240 %,
Temperature 90.0 °C
1630 psi

@Strain 0.240 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G33HS1L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin with outstanding impact resistance developed usin..
Tensile Stress 11.24 MPa

@Strain 0.200 %,
Temperature 100 °C
1630 psi

@Strain 0.200 %,
Temperature 212 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® HTN FR52G20NH BK337 Polyphthalamide (PPA)
Zytel® HTNFR52G20NH BK337 is a 20% glass reinforced, flame retardant, lubricated high performance polyamide resin. It is also a PPA resin and it uses a non-halogenated flame retardant.Information p..
Tensile Stress 11.24 MPa

@Strain 1.36 %,
Temperature 40.0 °C
1630 psi

@Strain 1.36 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC3090 NC010 Nylon 610  (Unverified Data**)
Unreinforced Renewably Sourced High Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3090 NC010 is a renewable sourced polyamide 610 containing a miniumu of 60% renewably sourced ingredien..