Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 12.27 MPa @Strain 0.250 %, Temperature 90.0 °C |
1780 psi @Strain 0.250 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® RE5329 BK503 Polyethylene Terephthalate (PET)
(Unverified Data**) 36% Glass Reinforced Polyethylene TerephthalateInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.3 MPa @Strain 0.450 %, Temperature 23.0 °C |
1780 psi @Strain 0.450 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® BM73G15THS BK317 Nylon 6
(Unverified Data**) 15% Glass Reinforced Heat Stabilized Polyamide 6 Zytel BM73G15THS is a 15% glass fiber reinforced heat stabilized lubricated toughened polyamide 6 for blow molding.Information provided by DuPont Per.. |