Mechanical Properties Metric English Comments
Tensile Stress 133.68 MPa

@Strain 1.66 %,
Temperature 40.0 °C
19389 psi

@Strain 1.66 %,
Temperature 104 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® 70G35HSLRA4 BK267 Nylon 66  (Unverified Data**)
Zytel® 70G35HSLRA4 BK267 is a 35% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding. It has excellent flow characteristics.Information provided ..
Tensile Stress 133.68 MPa

@Strain 3.33 %,
Temperature -40.0 °C
19389 psi

@Strain 3.33 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 73M40 NC010 Nylon 6  (Unverified Data**)
40% Mineral Reinforced Polyamide 6 Minlon 73M40 NC010 is a 40% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro..