Mechanical Properties Metric English Comments
Tensile Stress 2.22 MPa

@Strain 300 %
322 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® C4750 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Stress 2.22 MPa

@Strain 300 %
322 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® N8860 TPE, Nylon Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInformation from Alliance Polymers & Se..
Tensile Stress 2.22 MPa

@Strain 300 %
322 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P1957TB TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 2.22 MPa

@Strain 100 %
322 psi

@Strain 100 %
Average; ASTM D412 Method A
Seals Eastern 5722A Fluorocarbon-Elastomer
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Exce..
Tensile Stress 2.22 MPa

@Strain 0.100 %,
Temperature 23.0 °C
322 psi

@Strain 0.100 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)  (Unverified Data**)
Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also..