Polymer Property : Tensile Stress = 2.60 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 2.60 MPa

@Strain 300 %
377 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S KG 50A-3S2017 Thermoplastic Elastomer (TPE)
OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p..
Tensile Stress 2.60 MPa

@Strain 100 %
377 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P2765 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 2.60 MPa

@Strain 100 %
377 psi

@Strain 100 %
ASTM D412
Lubrizol ESTAGRIP® ST70A Polyether-Type Thermoplastic Polyurethane
Features: Low durometer soft feel for excellent grip; outstanding adhesionUses: Injection Molding - OvermoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation provided..
Tensile Stress 2.60 MPa

@Strain 10.0 %
377 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® XG6029 TPC-ET
Extrusion Grade
Tensile Stress 2.60 MPa

@Strain 26.51 %,
Temperature 120 °C
377 psi

@Strain 26.51 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 2.60 MPa

@Strain 0.130 %,
Temperature -40.0 °C
377 psi

@Strain 0.130 %,
Temperature -40.0 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010  (Unverified Data**)
Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s..
Tensile Stress 2.60 MPa

@Strain 108.07 %,
Temperature 90.0 °C
377 psi

@Strain 108.07 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 2.60 MPa

@Strain 10.0 %,
Temperature 23.0 °C
377 psi

@Strain 10.0 %,
Temperature 73.4 °F
ASTM D638
DuPont Performance Polymers Hytrel® G3548L TPC-ET  (Unverified Data**)
Hytrel® G3548L is a low modulus grade with nominal hardness of 35D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injec..
Tensile Stress 2.60 MPa

@Strain 6.00 %,
Temperature 40.0 °C
377 psi

@Strain 6.00 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..
Tensile Stress 2.60 MPa

@Strain 11.77 %,
Temperature 90.0 °C
377 psi

@Strain 11.77 %,
Temperature 194 °F
ISO 527
DuPont Performance Polymers Hytrel® G4078W TPC-ET  (Unverified Data**)
Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject..
Copyright © lookpolymers.com All Rights Reserved