Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 2.80 MPa

@Strain 300 %
406 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S KE 40A-3S1727 Thermoplastic Elastomer (TPE)
OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p..
Tensile Stress 2.80 MPa

@Strain 100 %
406 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® F02-137D TPE, Halogen Free Extrusion Grade
Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to..
Tensile Stress 2.80 MPa

@Strain 0.100 %,
Temperature -40.0 °C
406 psi

@Strain 0.100 %,
Temperature -40.0 °F
ISO 11403-1/-2
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer
Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided ..
Tensile Stress 2.80 MPa

@Strain 36.92 %,
Temperature 120 °C
406 psi

@Strain 36.92 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers
Tensile Stress 2.80 MPa

@Strain 0.220 %,
Temperature -20.0 °C
406 psi

@Strain 0.220 %,
Temperature -4.00 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET  (Unverified Data**)
65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers
Tensile Stress 2.80 MPa

@Strain 50.0 %,
Temperature 100 °C
406 psi

@Strain 50.0 %,
Temperature 212 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET  (Unverified Data**)
Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio..