Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 20.25 MPa @Strain 0.280 %, Temperature 90.0 °C |
2937 psi @Strain 0.280 %, Temperature 194 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK609 NC010 PBT
(Unverified Data**) Crastin® SK609 NC010 is a 50% glass fiber reinforced, lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 20.25 MPa @Strain 2.60 %, Temperature 80.0 °C |
2937 psi @Strain 2.60 %, Temperature 176 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® FR7026V0F BK001 Nylon 66
(Unverified Data**) Zytel® FR7026V0F BK001 is a flame retardant heat stabilized polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuP.. |