Tensile Stress 20.25 MPa

@Strain 0.280 %,
Temperature 90.0 °C
2937 psi

@Strain 0.280 %,
Temperature 194 °F
ISO 527
DuPont Performance Polymers Crastin® SK609 NC010 PBT  (Unverified Data**)
Crastin® SK609 NC010 is a 50% glass fiber reinforced, lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 20.25 MPa

@Strain 2.60 %,
Temperature 80.0 °C
2937 psi

@Strain 2.60 %,
Temperature 176 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® FR7026V0F BK001 Nylon 66  (Unverified Data**)
Zytel® FR7026V0F BK001 is a flame retardant heat stabilized polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuP..