Polymer Property : Tensile Stress = 20.91 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 20.91 MPa

@Strain 0.200 %,
Temperature 23.0 °C
3033 psi

@Strain 0.200 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G33HS1L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor..
Tensile Stress 20.91 MPa

@Strain 33.17 %,
Temperature 40.0 °C
3033 psi

@Strain 33.17 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1600 NC010 Nylon 1010
Plasticized Toughened UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1600 NC010 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced..