Mechanical Properties Metric English Comments
Tensile Stress 1.52 MPa

@Strain 100 %,
Temperature 23.0 °C
220 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ CL2250 Thermoplastic Elastomer (TPE)
Versaflex™ CL2250 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov..
Tensile Stress 1.52 MPa

@Strain 100 %
220 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P2950 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 1.52 MPa

@Strain 100 %,
Temperature 23.0 °C
220 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G2755-1000-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G2755-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypro..
Tensile Stress 1.52 MPa

@Strain 100 %,
Temperature 23.0 °C
220 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7650-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7650-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
Tensile Stress 1.52 MPa

@Strain 100 %,
Temperature 23.0 °C
220 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7650-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7650-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
Tensile Stress 1.52 MPa

@Strain 5.88 %,
Temperature 100 °C
220 psi

@Strain 5.88 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..