Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 225 MPa @Strain 0.500 %, Temperature 1204 °C |
32600 psi @Strain 0.500 %, Temperature 2199 °F |
|
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |