Tensile Stress 24.0 MPa

@Strain 50.0 %,
Temperature 23.0 °C
3480 psi

@Strain 50.0 %,
Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Hytrel® 7246HS BK320 TPC-ET  (Unverified Data**)
Hytrel® 7246HS BK320 is a high modulus, heat stabilized, black grade with nominal hardness of 72D.Information provided by DuPont
Tensile Stress 24.0 MPa

@Strain 30.0 %,
Temperature 150 °C
3480 psi

@Strain 30.0 %,
Temperature 302 °F
Solvay TECHNYL® A 205F PA66, DRY
Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities..
Tensile Stress 24.0 MPa

@Strain 50.0 %
3480 psi

@Strain 50.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers
Tensile Stress 24.0 MPa

@Strain 50.0 %
3480 psi

@Strain 50.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 24.0 MPa

@Strain 50.0 %
3480 psi

@Strain 50.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 7246HS BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers
Tensile Stress 24.0 MPa

@Strain 100 %
3480 psi

@Strain 100 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR8730 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Viscosity Polyester Elastomer with Excellent Mechanical Properties at Elevated Temperatures Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 24.0 MPa

@Time 3600 sec,
Strain 3.29603 %
3480 psi

@Time 1.00 hour,
Strain 3.29603 %
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 101L NC010 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101L NC010 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 24.0 MPa

@Strain 3.91667 %,
Time 36000 sec
3480 psi

@Strain 3.91667 %,
Time 10.0 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 101L NC010 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101L NC010 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 24.0 MPa

@Strain 100 %
3480 psi

@Strain 100 %
ASTM D412
Alliance Polymers Zythane™ 6055D Thermoplastic Polyurethane Elastomer
Zythane™ 6055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress 24.0 MPa

@Strain 100 %
3480 psi

@Strain 100 %
ASTM D412
Alliance Polymers Zythane™ 7055D Thermoplastic Polyurethane Elastomer
Zythane™ 7055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress >= 24.0 MPa

@Strain 300 %
>= 3480 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 298A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Tensile Stress 24.0 MPa

@Strain 50.0 %,
Temperature 150 °C
3480 psi

@Strain 50.0 %,
Temperature 302 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66  (Unverified Data**)
Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi..
Tensile Stress 24.0 MPa

@Strain 50.0 %,
Temperature 23.0 °C
3480 psi

@Strain 50.0 %,
Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Hytrel® 7246HS NC010 TPC-ET  (Unverified Data**)
Hytrel® 7246HS NC010 is a high modulus, heat stabilized grade with nominal hardness of 72D.Information provided by DuPont