DuPont Performance Polymers Hytrel® HTR8730 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)

Category Polymer , Thermoplastic , Polyester, TP , Polyester Thermoplastic Elastomer
Manufacturer DuPont Performance Polymers
Trade Name Hytrel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Hytrel® HTR8730 BK320 Polyester Elastomer TPC-ET  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
63 Shore D High Viscosity Polyester Elastomer with Excellent Mechanical Properties at Elevated Temperatures Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
1.20 g/cc
0.0434 lb/in³
ISO 1183
Water Absorption 0.50 %

@Thickness 2.00 mm
0.50 %

@Thickness 0.0787 in
DS; Sim. to ISO 62
Moisture Absorption 0.200 %

@Thickness 2.00 mm
0.200 %

@Thickness 0.0787 in
DS; Sim. to ISO 62
Water Absorption at Saturation 0.30 %
0.30 %
Immersion 24h; ASTM D570
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.021 cm/cm
0.021 in/in
ISO 294-4 2577
Melt Flow 5.0 g/10 min

@Load 10.0 kg,
Temperature 230 °C
5.0 g/10 min

@Load 22.0 lb,
Temperature 446 °F
cm³/10min; ISO 1133
5.0 g/10 min

@Load 10.0 kg,
Temperature 230 °C
5.0 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
15s; ISO 868
Tensile Strength at Break 41.0 MPa
5950 psi
ISO 527-1/-2
Tensile Stress 10.0 MPa

@Strain 5.00 %
1450 psi

@Strain 5.00 %
ISO 527-1/-2
15.0 MPa

@Strain 10.0 %
2180 psi

@Strain 10.0 %
ISO 527-1/-2
22.0 MPa

@Strain 50.0 %
3190 psi

@Strain 50.0 %
ISO 527-1/-2
24.0 MPa

@Strain 100 %
3480 psi

@Strain 100 %
ISO 527-1/-2
Elongation at Break >= 300 %
>= 300 %
ISO 527-1/-2
450 %
450 %
Nominal; ISO 527-1/-2
Tensile Modulus 0.270 GPa
39.2 ksi
ISO 527-1/-2
Flexural Modulus 0.290 GPa
42.1 ksi
ISO 178
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched NB
NB
ISO 179/1eA
1.00 J/cm²

@Temperature -40.0 °C
4.76 ft-lb/in²

@Temperature -40.0 °F
ISO 179/1eA
1.40 J/cm²

@Temperature -30.0 °C
6.66 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Tear Strength 150 kN/m
856 pli
normal; ISO 34-1
180 kN/m
1030 pli
parallel; ISO 34-1
Thermal Properties Metric English Comments
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1/-3
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
IEC 60695-11-10
Descriptive Properties Value Comments
Delivery Form Pellets
Part Marking Code >TPC-ET<
ISO 11469
Processing Blow Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification TPC-ET
ISO 1043
Special Characteristics Heat stabilised or stable to heat
Light stabilised or stable to light
Users viewing this material also viewed the following: