Polymer Property : Tensile Stress = 24.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 24.6 MPa

@Strain 0.900 %,
Temperature 23.0 °C
3570 psi

@Strain 0.900 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper..
Tensile Stress 24.6 MPa

@Strain 0.900 %,
Temperature 23.0 °C
3570 psi

@Strain 0.900 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration ..
Tensile Stress 24.6 MPa

@Strain 6.00 %,
Temperature 150 °C
3570 psi

@Strain 6.00 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 11C40 NC010 Nylon 66  (Unverified Data**)
40% Mineral Reinforced Polyamide 66 Minlon 11C40 NC010 is a 40% mineral reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers