Polymer Property : Tensile Stress = 2441 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 16.83 MPa

@Strain 0.120 %,
Temperature 0.000 °C
2441 psi

@Strain 0.120 %,
Temperature 32.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FE350064 BK544 Polyphthalamide (PPA)  (Unverified Data**)
Carbon Fiber Reinforced Toughened PPA High Performance Polyamide Zytel HTNFE350064 BK544 is a carbon fiber reinforced toughened heat stabilized conductive high performance polyamide resin developed ..