Mechanical Properties Metric English Comments
Tensile Stress 1.80 MPa

@Strain 100 %
261 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S FR 60A-3S1846 Thermoplastic Elastomer (TPE)
OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo..
Tensile Stress 1.80 MPa

@Strain 300 %,
Temperature 23.0 °C
261 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ OM 9-801N Thermoplastic Elastomer (TPE)
Versaflex™ OM 9-801N is designed for overmolding onto a wide variety of substrates including PC, ABS, PC/ABS, HIPS, PPO, acetal, acrylic and copolyester. - Bonds to a Variety Of Substrates - Rubber..
Tensile Stress 1.80 MPa

@Strain 100 %
261 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P3953CT TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 1.80 MPa

@Strain 10.0 %
261 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b..
Tensile Stress 1.80 MPa

@Strain 10.0 %,
Temperature 23.0 °C
261 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b..
Tensile Stress 1.80 MPa

@Strain 0.281 %,
Time 360000 sec
261 psi

@Strain 0.281 %,
Time 100 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6  (Unverified Data**)
Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 1.80 MPa

@Strain 0.308 %,
Time 3.60e+6 sec
261 psi

@Strain 0.308 %,
Time 1000 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6  (Unverified Data**)
Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 1.80 MPa

@Strain 0.182 %,
Time 3600 sec
261 psi

@Strain 0.182 %,
Time 1.00 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6  (Unverified Data**)
Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 1.80 MPa

@Strain 10.0 %,
Temperature 100 °C
261 psi

@Strain 10.0 %,
Temperature 212 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET  (Unverified Data**)
Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio..
Tensile Stress 1.80 MPa

@Strain 100 %
261 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ P50A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P50A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 1.80 MPa

@Strain 100 %
261 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ P50A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P50A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..