Polymer Property : Tensile Stress = 262 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 262 MPa

@Strain 0.200 %
38000 psi

@Strain 0.200 %
Process Temperature T3
COI Ceramics Sylramic™ S300 Silicon Carbide Ceramic Matrix Composite, SiC
Description: Engineered ceramic composite structures for a broad range of industries and applications.Reinforcing Fiber Flexibility: S300 - Sylramic SiC Preceramic Polymer Matrix Precursors: S300 - ..
Tensile Stress 262 MPa

@Strain 0.00500 %
38000 psi

@Strain 0.00500 %
COI Ceramics Sylramic™ S400 Silicon Carbide Ceramic Matrix Composite, Carbon
Description: Engineered ceramic composite structures for a broad range of industries and applications.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crysta..