Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

COI Ceramics Sylramic™ S400 Silicon Carbide Ceramic Matrix Composite, Carbon

Category Ceramic , Carbide , Ceramic Matrix Composite
Manufacturer COI Ceramics
Trade Name Sylramic™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF COI Ceramics Sylramic™ S400 Silicon Carbide Ceramic Matrix Composite, Carbon.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Engineered ceramic composite structures for a broad range of industries and applications.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix (
Physical Properties Metric English Comments
Bulk Density 2.10 g/cc
0.0759 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength 5.52 MPa
801 psi
Interlaminar
290 MPa
42100 psi
Tensile Stress 86.2 MPa

@Strain 0.00100 %
12500 psi

@Strain 0.00100 %
134 MPa

@Strain 0.00200 %
19500 psi

@Strain 0.00200 %
159 MPa

@Strain 0.00300 %
23000 psi

@Strain 0.00300 %
207 MPa

@Strain 0.00400 %
30000 psi

@Strain 0.00400 %
262 MPa

@Strain 0.00500 %
38000 psi

@Strain 0.00500 %
303 MPa

@Strain 0.00600 %
44000 psi

@Strain 0.00600 %
Tensile Strength, Yield 98.6 MPa
14300 psi
Elongation at Break 0.53 %
0.53 %
Tensile Modulus 110 GPa
16000 ksi
Flexural Strength 241 MPa
35000 psi
4 point
Shear Strength 27.6 MPa
4000 psi
Short Beam
Thermal Properties Metric English Comments
CTE, linear 2.60 µm/m-°C

@Temperature 20.0 - 1200 °C
1.44 µin/in-°F

@Temperature 68.0 - 2190 °F
Descriptive Properties Value Comments
Nominal Fiber Volume (%) 40