Mechanical Properties Metric English Comments
Tensile Stress 20.6 MPa

@Strain 35.0 %,
Temperature 0.000 °C
2990 psi

@Strain 35.0 %,
Temperature 32.0 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 20.6 MPa

@Strain 40.0 %,
Temperature 0.000 °C
2990 psi

@Strain 40.0 %,
Temperature 32.0 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 20.6 MPa

@Strain 45.0 %,
Temperature 0.000 °C
2990 psi

@Strain 45.0 %,
Temperature 32.0 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 20.6 MPa

@Strain 50.0 %,
Temperature 0.000 °C
2990 psi

@Strain 50.0 %,
Temperature 32.0 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 20.6 MPa

@Strain 10.3 %,
Temperature 90.0 °C
2990 psi

@Strain 10.3 %,
Temperature 194 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers