Polymer Property : Tensile Stress = 3.10 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 3.10 MPa

@Strain 300 %
450 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S EH 60A-3S7003 Thermoplastic Elastomer (TPE)
OnFlex™-S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t..
Tensile Stress 3.10 MPa

@Strain 300 %
450 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S FR 40A-3S1841 Thermoplastic Elastomer (TPE)
OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo..
Tensile Stress 3.10 MPa

@Strain 100 %
450 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® C4970M TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Stress 3.10 MPa

@Strain 100 %,
Temperature 23.0 °C
450 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ HC MT317 Thermoplastic Elastomer (TPE)
Versaflex™ HC MT317 is an extrudable, sterilizable TPE developed for medical tubing applications in healthcare. - Autoclavable sterilizable - Flexible - Kink Resistant New product. Commercial speci..
Tensile Stress 3.10 MPa

@Strain 300 %,
Temperature 23.0 °C
450 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7970-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7970-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Tensile Stress 3.10 MPa

@Strain 300 %
450 psi

@Strain 300 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ EG-9065 Thermoplastic Elastomer (TPE)
The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compoun..
Tensile Stress 3.10 MPa

@Strain 300 %,
Temperature 23.0 °C
450 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7970-1 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7970-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Tensile Stress 3.10 MPa

@Strain 300 %,
Temperature 23.0 °C
450 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7970-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7970-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
Tensile Stress 3.10 MPa

@Strain 300 %,
Temperature 23.0 °C
450 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7970-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
Tensile Stress 3.10 MPa

@Strain 100 %
450 psi

@Strain 100 %
ASTM D412
Teknor Apex Telcar® TELC 302 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Stress 3.10 MPa

@Strain 100 %
450 psi

@Strain 100 %
ASTM D412
Teknor Apex Telcar® TL-4001A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Stress 3.10 MPa

@Strain 0.100 %,
Temperature 60.0 °C
450 psi

@Strain 0.100 %,
Temperature 140 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® FR7026V0F BK001 Nylon 66  (Unverified Data**)
Zytel® FR7026V0F BK001 is a flame retardant heat stabilized polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuP..
Tensile Stress 3.10 MPa

@Strain 0.150 %,
Temperature -20.0 °C
450 psi

@Strain 0.150 %,
Temperature -4.00 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610  (Unverified Data**)
Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie..
Tensile Stress 3.10 MPa

@Strain 300 %
450 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ P50A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P50A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 3.10 MPa

@Strain 300 %
450 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ P50A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P50A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 3.10 MPa

@Strain 100 %
450 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ P75A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P75A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 3.10 MPa

@Strain 100 %
450 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ P75A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P75A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..