Polymer Property : Tensile Stress = 3.40 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 3.40 MPa

@Strain 300 %
493 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P2765 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 3.40 MPa

@Strain 0.200 %,
Temperature 80.0 °C
493 psi

@Strain 0.200 %,
Temperature 176 °F
ISO 11403-1/-2
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer
Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided ..
Tensile Stress 3.40 MPa

@Strain 26.8 %,
Temperature 90.0 °C
493 psi

@Strain 26.8 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 3.40 MPa

@Strain 74.01 %,
Temperature 120 °C
493 psi

@Strain 74.01 %,
Temperature 248 °F
ISO 527
DuPont Performance Polymers Hytrel® G4078W TPC-ET  (Unverified Data**)
Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject..
Tensile Stress 3.40 MPa

@Strain 5.00 %,
Temperature 23.0 °C
493 psi

@Strain 5.00 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET  (Unverified Data**)
Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio..
Tensile Stress 3.40 MPa

@Strain 300 %
493 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ G65A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G65A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 3.40 MPa

@Strain 300 %
493 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ G65A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G65A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 3.40 MPa

@Strain 100 %
493 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ G80A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G80A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 3.40 MPa

@Strain 100 %
493 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ G80A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G80A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 3.40 MPa

@Strain 100 %
493 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ P55A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P55A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress >= 3.40 MPa

@Strain 100 %
>= 493 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 382A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tensile Stress 3.40 MPa

@Strain 100 %
493 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ P55A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P55A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..