Tensile Stress 3.60 MPa

@Strain 300 %
522 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S EF 70A-3S1975 Thermoplastic Elastomer (TPE)
OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell..
Tensile Stress 3.60 MPa

@Strain 300 %
522 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S FR 50A-3S1831 Thermoplastic Elastomer (TPE)
OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo..
Tensile Stress 3.60 MPa

@Strain 300 %
522 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S HF 70A-3S1984 Thermoplastic Elastomer (TPE)
OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu..
Tensile Stress 3.60 MPa

@Strain 100 %
522 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S HF 90A-3S1988 Thermoplastic Elastomer (TPE)
OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu..
Tensile Stress 3.60 MPa

@Strain 47.25 %,
Temperature 100 °C
522 psi

@Strain 47.25 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 3.60 MPa

@Strain 150.02 %,
Temperature 120 °C
522 psi

@Strain 150.02 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers
Tensile Stress 3.60 MPa

@Strain 23.55 %,
Temperature 90.0 °C
522 psi

@Strain 23.55 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..
Tensile Stress 3.60 MPa

@Strain 98.4 %,
Temperature 120 °C
522 psi

@Strain 98.4 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..
Tensile Stress 3.60 MPa

@Strain 300 %
522 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ G70A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G70A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 3.60 MPa

@Strain 300 %
522 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ G70A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G70A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 3.60 MPa

@Strain 300 %
522 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 3.60 MPa

@Strain 300 %
522 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ P60A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P60A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 3.60 MPa

@Strain 100 %
522 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ P80A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P80A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 3.60 MPa

@Strain 100 %
522 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ P80A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P80A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..