Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 2.07 MPa

@Strain 100 %
300 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P3862 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 2.07 MPa

@Strain 300 %,
Temperature 23.0 °C
300 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G2712-1000-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G2712-1000-02 is an easy processing TPE designed for injection molding and extrusion aplications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - High..
Tensile Stress >= 2.07 MPa

@Strain 50.0 %
>= 300 psi

@Strain 50.0 %
ASTM D412 Method A
Seals Eastern 7346 Extreme Low Temperature Service Rubber
HNBR for cold temp (-50°C) and/or aqueous serviceInformation provided by Seals Eastern.
Tensile Stress 2.07 MPa

@Strain 100 %
300 psi

@Strain 100 %
ASTM D412
Teknor Apex Telcar® TL-1522A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Stress 2.07 MPa

@Strain 0.100 %,
Temperature -40.0 °C
300 psi

@Strain 0.100 %,
Temperature -40.0 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010  (Unverified Data**)
Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s..
Tensile Stress 2.07 MPa

@Strain 82.96 %,
Temperature 200 °C
300 psi

@Strain 82.96 %,
Temperature 392 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET  (Unverified Data**)
65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers
Tensile Stress 2.07 MPa

@Strain 0.160 %,
Temperature -20.0 °C
300 psi

@Strain 0.160 %,
Temperature -4.00 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET  (Unverified Data**)
65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved