Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Dynaflex™ G2712-1000-02 Thermoplastic Elastomer (TPE)

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer PolyOne Corporation
Trade Name Dynaflex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Dynaflex™ G2712-1000-02 Thermoplastic Elastomer (TPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dynaflex™ G2712-1000-02 is an easy processing TPE designed for injection molding and extrusion aplications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - High Flow For Thin-Wall Parts - Overmold Adhesion to Polypropylene - Rubbery Feel - Soft TouchDynaflex™ G2712-1000-02 can be recycled as a filler or impact modifier for polyolefins, or can be recycled by grinding and reintroduction to the molding process. Similar to PP or PE recycling process, if separated appropriately, it can be recycled many times. Municipality waste stream recycle code is 7 which is designated for Other. Please contact GLS Thermoplastic Elastomers for a copy of our Recyclability Compliance letter.Color concentrates with polypropylene (PP), ethylene vinyl acetate (EVA), or low density polyethylene (PE) carrier are most suitable for coloring Dynaflex™ G2712-1000-02. Improved color dispersion can be achieved by using higher melt flow concentrates (with a melt flow from 20 - 40 g/10 min). Typical loadings for color concentrates are 1% to 5% by weight. Liquid color can be used, but mineral oil based carriers may have a significant effect on the final hardness value. Concentrates based on PVC should not be used. A high color match consistency can be obtained by using precolored compounds available from GLS. The final determination of color concentrate suitability should be determined by customer trials. Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP). Regrind levels up to 20% can be used with Dynaflex™ G2712-1000-02 with minimal property loss, provided that the regrind is free of contamination. To minimize losses during molding, the melt temperature should remain as low as possible. The final determination of regrind effectiveness should be determined by the customer. Dynaflex™ G2712-1000-02 has excellent melt stability. Maximum residence times may vary, depending on the size of the barrel. Generally, the barrel should be emptied if it is idle for periods of 8 - 10 minutes or longer. Drying is not Required Injection Speed: 1 to 5 in/sec 1st Stage - Boost Pressure: 100 to 500 psi 2nd Stage - Hold Pressure: 70% of Boost Hold Time (Thick Part): 4 to 10 sec Hold Time (Thin Part): 1 to 3 secInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 0.888 g/cc
0.888 g/cc
ASTM D792
Viscosity 8900 cP

@Shear Rate 11200 1/s,
Temperature 200 °C
8900 cP

@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
Linear Mold Shrinkage, Flow 0.013 - 0.019 cm/cm
0.013 - 0.019 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 43
43
10 sec; ASTM D2240
Tensile Strength at Break 5.65 MPa

@Temperature 23.0 °C
819 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tensile Stress 1.31 MPa

@Strain 100 %,
Temperature 23.0 °C
190 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
2.07 MPa

@Strain 300 %,
Temperature 23.0 °C
300 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 700 %

@Temperature 23.0 °C
700 %

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tear Strength 19.3 kN/m
110 pli
ASTM D624
Compression Set 17 %

@Temperature 23.0 °C,
Time 79200 sec
17 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B
Processing Properties Metric English Comments
Rear Barrel Temperature 149 - 177 °C
300 - 351 °F
Middle Barrel Temperature 171 - 188 °C
340 - 370 °F
Front Barrel Temperature 182 - 221 °C
360 - 430 °F
Nozzle Temperature 182 - 221 °C
360 - 430 °F
Mold Temperature 15.6 - 26.7 °C
60.1 - 80.1 °F
Back Pressure 0.345 - 1.03 MPa
50.0 - 149 psi
Screw Speed 25 - 75 rpm
25 - 75 rpm
Descriptive Properties Value Comments
Agency Ratings FDA 21 CFR 177.1210
Please contact GLS Thermoplastic Elastomers for a copy of the FDA compliance letter.
Appearance Translucent
Features Good Colorability
Good UV Resistance
High Flow
Ozone Resistant
Recyclable Material
Forms Pellets
Generic Material TPE
Generic Name Thermoplastic Elastomer (TPE)
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Suggested Max Regrind 20%
Uses Consumer Applications
Overmolding
Personal Care
Thin-walled Parts
Transparent or Translucent Parts
Users viewing this material also viewed the following: