Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 34800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 240 MPa

@Strain 2.00 %
34800 psi

@Strain 2.00 %
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY
Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 240 MPa

@Diameter 105 - 200 mm,
Strain 0.200 %
34800 psi

@Diameter 4.13 - 7.87 in,
Strain 0.200 %
United Cast Bar Unibar 400-15 As Cast Continuously Cast Spheroidal Graphite Iron
Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend..
Tensile Stress 240 MPa

@Diameter 205 - 600 mm,
Strain 0.200 %
34800 psi

@Diameter 8.07 - 23.6 in,
Strain 0.200 %
United Cast Bar Unibar 400-15 As Cast Continuously Cast Spheroidal Graphite Iron
Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend..
Tensile Stress 240 MPa

@Diameter 105 - 200 mm,
Strain 0.200 %
34800 psi

@Diameter 4.13 - 7.87 in,
Strain 0.200 %
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron
Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend..
Tensile Stress 240 MPa

@Diameter 205 - 600 mm,
Strain 0.200 %
34800 psi

@Diameter 8.07 - 23.6 in,
Strain 0.200 %
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron
Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend..
Tensile Stress 240 MPa

@Strain 0.500 %,
Temperature 982 °C
34800 psi

@Strain 0.500 %,
Temperature 1800 °F
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon
Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix (
Copyright © lookpolymers.com All Rights Reserved