Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 26.8 MPa @Strain 3.20 %, Temperature 90.0 °C |
3890 psi @Strain 3.20 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 300PE BK602 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE BK602 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low.. |
|||
Tensile Stress | 26.8 MPa @Strain 3.80 %, Temperature 90.0 °C |
3890 psi @Strain 3.80 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Tensile Stress | 26.8 MPa @Strain 1.85 %, Temperature 23.0 °C |
3890 psi @Strain 1.85 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers |