Polymer Property : Tensile Stress = 4.50 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 4.50 MPa

@Strain 100 %,
Thickness 2.00 mm
653 psi

@Strain 100 %,
Thickness 0.0787 in
Type 1, 200 mm/min; Flow; DIN 53504
PolyOne OnFlex™ BIO 5380A-E0006 Thermoplastic Elastomer (TPE)
OnFlex™ BIO 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi..
Tensile Stress 4.50 MPa

@Strain 300 %
653 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S EH 80A-3S7005 Thermoplastic Elastomer (TPE)
OnFlex™ S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t..
Tensile Stress 4.50 MPa

@Strain 300 %
653 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S KE 60A-3S1725 Thermoplastic Elastomer (TPE)
OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p..
Tensile Stress 4.50 MPa

@Strain 300 %
653 psi

@Strain 300 %
ASTM D412
Lubrizol ESTAGRIP® ST70A Polyether-Type Thermoplastic Polyurethane
Features: Low durometer soft feel for excellent grip; outstanding adhesionUses: Injection Molding - OvermoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation provided..
Tensile Stress 4.50 MPa

@Strain 100 %
653 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® XG6029 TPC-ET
Extrusion Grade
Tensile Stress 4.50 MPa

@Strain 0.180 %,
Temperature 90.0 °C
653 psi

@Strain 0.180 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Tensile Stress 4.50 MPa

@Strain 0.180 %,
Temperature 90.0 °C
653 psi

@Strain 0.180 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HFS NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Tensile Stress 4.50 MPa

@Strain 300 %
653 psi

@Strain 300 %
ASTM D412
ExxonMobil Vistamaxx™ 3000 Propylene-based Elastomer
Product Description: Vistamaxx 3000 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Technology. It has moderate elastomeric properties, is easy to ..
Tensile Stress 4.50 MPa

@Strain 5.00 %
653 psi

@Strain 5.00 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET  (Unverified Data**)
44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin..
Tensile Stress 4.50 MPa

@Strain 200 %,
Temperature 100 °C
653 psi

@Strain 200 %,
Temperature 212 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET  (Unverified Data**)
Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio..
Tensile Stress >= 4.50 MPa

@Strain 300 %
>= 653 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 270A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Tensile Stress >= 4.50 MPa

@Strain 300 %
>= 653 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 465A Polyester-based TPU
Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Stress >= 4.50 MPa

@Strain 100 %
>= 653 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 470A Polyester-based TPU
Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech