Mechanical Properties Metric English Comments
Tensile Stress 28.29 MPa

@Strain 0.230 %,
Temperature -20.0 °C
4103 psi

@Strain 0.230 %,
Temperature -4.00 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FE350064 BK544 Polyphthalamide (PPA)  (Unverified Data**)
Carbon Fiber Reinforced Toughened PPA High Performance Polyamide Zytel HTNFE350064 BK544 is a carbon fiber reinforced toughened heat stabilized conductive high performance polyamide resin developed ..
Tensile Stress 28.29 MPa

@Strain 4.85 %,
Temperature 40.0 °C
4103 psi

@Strain 4.85 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6  (Unverified Data**)
30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro..