Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 46.0 MPa @Strain 29.0 %, Temperature 40.0 °C |
6670 psi @Strain 29.0 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers |