Mechanical Properties Metric English Comments
Tensile Stress 46.09 MPa

@Strain 0.790 %,
Temperature -20.0 °C
6685 psi

@Strain 0.790 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Tensile Stress 46.09 MPa

@Strain 0.790 %,
Temperature -20.0 °C
6685 psi

@Strain 0.790 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HFS NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Tensile Stress 46.09 MPa

@Strain 3.43 %,
Temperature 150 °C
6685 psi

@Strain 3.43 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 540SUV BK544 Polyethylene Terephthalate (PET)  (Unverified Data**)
40% Glass Reinforced UV Stabilized Polyethylene Terephthalate Developed for Extrusion and Injection Molding Rynite 540SUV BK544 is a 40% glass fiber reinforced UV stabilized modified polyethylene te..
Tensile Stress 46.09 MPa

@Strain 0.480 %,
Temperature 0.000 °C
6685 psi

@Strain 0.480 %,
Temperature 32.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® FE270038 BK267 Nylon 66  (Unverified Data**)
40% Glass/Mineral Reinforced Polyamide 66 Zytel FE270038 is a 40% glass fiber/mineral reinforced heat stabilized polyamid 66 for injection molding. It is well suited for water injection technology.I..
Tensile Stress 46.09 MPa

@Strain 20.01 %,
Temperature 40.0 °C
6685 psi

@Strain 20.01 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)  (Unverified Data**)
Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also..