Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 32.6 MPa @Strain 11.4 %, Temperature 90.0 °C |
4730 psi @Strain 11.4 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500CL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL is a medium viscosity acetal homopolymer resin containing a chemical lubricant designed for low wear and fr.. |