Mechanical Properties Metric English Comments
Tensile Stress 3.35 MPa

@Strain 100 %
486 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® A9855B TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
Tensile Stress 3.35 MPa

@Strain 100 %,
Temperature 21.0 °C
486 psi

@Strain 100 %,
Temperature 69.8 °F
Across Flow 2 hr; ASTM D412
PolyOne Versalloy™ HC 9220-80 Thermoplastic Elastomer (TPE)
Versalloy™ HC 9220-80 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr..
Tensile Stress 3.35 MPa

@Strain 0.0700 %,
Temperature 150 °C
486 psi

@Strain 0.0700 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 54G35EF BK420 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced Toughened PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN54G35EF BK420 is a 35% glass reinforced toughened heat stabilized lubrica..
Tensile Stress 3.35 MPa

@Strain 5.00 %,
Temperature 100 °C
486 psi

@Strain 5.00 %,
Temperature 212 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 3.35 MPa

@Strain 5.86 %,
Temperature 23.0 °C
486 psi

@Strain 5.86 %,
Temperature 73.4 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..