Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 33.79 MPa @Strain 1.00 %, Temperature 90.0 °C |
4901 psi @Strain 1.00 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® RE5329 BK503 Polyethylene Terephthalate (PET)
(Unverified Data**) 36% Glass Reinforced Polyethylene TerephthalateInformation provided by DuPont Performance Polymers |