Polymer Property : Tensile Stress = 4930 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 34.0 MPa

@Strain 20.0 %,
Temperature 23.0 °C
4930 psi

@Strain 20.0 %,
Temperature 73.4 °F
Solvay TECHNYL® A 205F PA66, Conditioned
Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities..
Tensile Stress 34.0 MPa

@Strain 10.0 %
4930 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET  (Unverified Data**)
82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 34.0 MPa

@Strain 0.580 %,
Temperature 150 °C
4930 psi

@Strain 0.580 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® PLS 95G50DH2 BK261 Nylon 6  (Unverified Data**)
50% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology only from DuPont providing exceptional Heat Resistanc..