Mechanical Properties Metric English Comments
Tensile Stress 5.10 MPa

@Strain 300 %
740 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S HF 90A-3S1988 Thermoplastic Elastomer (TPE)
OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu..
Tensile Stress 5.10 MPa

@Strain 100 %
740 psi

@Strain 100 %
ASTM D412
Teknor Apex Monprene® MP-1848K Thermoplastic Elastomer
Uses: Wire and Cable ApplicationsForms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to..
Tensile Stress 5.10 MPa

@Strain 25.0 %
740 psi

@Strain 25.0 %
Average; ASTM D412 Method A
Seals Eastern 7042 Fluorocarbon-Elastomer
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type..
Tensile Stress 5.10 MPa

@Strain 5.00 %
740 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® VT3108 TPC-ET
Extrusion Grade, High Breathable, Drying of Material Required
Tensile Stress 5.10 MPa

@Strain 100 %
740 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® EL250 TPC-ET
Injection Molding
Tensile Stress 5.10 MPa

@Strain 6.00 %,
Temperature 23.0 °C
740 psi

@Strain 6.00 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET  (Unverified Data**)
47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc..
Tensile Stress 5.10 MPa

@Strain 5.00 %,
Temperature 23.0 °C
740 psi

@Strain 5.00 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® HTR5612BK TPC-ET  (Unverified Data**)
Hytrel® HTR5612BK HTR5612BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal durometer hardness of 54D, is pigmented black with fine particle size..
Tensile Stress 5.10 MPa

@Strain 38.95 %,
Temperature 120 °C
740 psi

@Strain 38.95 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 5.10 MPa

@Strain 100 %
740 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ P85A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P85A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 5.10 MPa

@Strain 100 %
740 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ P85A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P85A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..