Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 34.61 MPa @Strain 1.68 %, Temperature 160 °C |
5020 psi @Strain 1.68 %, Temperature 320 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |
|||
Tensile Stress | 34.6 MPa @Strain 19.5 %, Temperature 40.0 °C |
5020 psi @Strain 19.5 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part.. |
|||
Tensile Stress | 34.6 MPa @Strain 1.45 %, Temperature 0.000 °C |
5020 psi @Strain 1.45 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers |