Mechanical Properties Metric English Comments
Tensile Stress 3.52 MPa

@Strain 300 %,
Temperature 23.0 °C
511 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versalloy™ HC 9210-70N Thermoplastic Elastomer (TPE)
Versalloy™ HC 9210-70N is a USP Class VI, TPV alloy targeted for injection molding healthcare applications such as disposable medical items and soft-touch overmolding for surgical grips. Product ex..
Tensile Stress 3.52 MPa

@Strain 300 %
511 psi

@Strain 300 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ EG-9072 Thermoplastic Elastomer (TPE)
The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compoun..
Tensile Stress 3.52 MPa

@Strain 200 %
511 psi

@Strain 200 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ EG-9165 Thermoplastic Elastomer (TPE)
The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun..
Tensile Stress 3.52 MPa

@Strain 86.68 %,
Temperature 100 °C
511 psi

@Strain 86.68 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 3.52 MPa

@Strain 3.88 %,
Temperature 90.0 °C
511 psi

@Strain 3.88 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers
Tensile Stress 3.52 MPa

@Strain 0.150 %,
Temperature 23.0 °C
511 psi

@Strain 0.150 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC3090 NC010 Nylon 610  (Unverified Data**)
Unreinforced Renewably Sourced High Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3090 NC010 is a renewable sourced polyamide 610 containing a miniumu of 60% renewably sourced ingredien..
Tensile Stress 3.52 MPa

@Strain 27.31 %,
Temperature 90.0 °C
511 psi

@Strain 27.31 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers
Tensile Stress 3.52 MPa

@Strain 16.75 %,
Temperature 60.0 °C
511 psi

@Strain 16.75 %,
Temperature 140 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers
Tensile Stress 3.52 MPa

@Strain 21.33 %,
Temperature 180 °C
511 psi

@Strain 21.33 %,
Temperature 356 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET  (Unverified Data**)
65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers