Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 5210 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 35.9 MPa

@Strain 1.90 %,
Temperature 40.0 °C
5210 psi

@Strain 1.90 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging..
Tensile Stress 35.9 MPa

@Strain 33.83 %,
Temperature 40.0 °C
5210 psi

@Strain 33.83 %,
Temperature 104 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1010 NC010 Nylon 1010  (Unverified Data**)
Unreinforced Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight. ..
Tensile Stress 35.9 MPa

@Strain 1.92 %,
Temperature 120 °C
5210 psi

@Strain 1.92 %,
Temperature 248 °F
ISO 527
DuPont Performance Polymers Rynite® 408 NC010 PET
Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf..
Tensile Stress 35.9 MPa

@Strain 0.250 %,
Temperature 23.0 °C
5210 psi

@Strain 0.250 %,
Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66
Information provided by DuPont Performance Polymers
Tensile Stress 35.9 MPa

@Strain 0.300 %,
Temperature 23.0 °C
5210 psi

@Strain 0.300 %,
Temperature 73.4 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66  (Unverified Data**)
Zytel® 80G43HS1L BK104 is a 43% glass fiber reinforced, heat stabilized, black polyamide 66 resin with superior impact resistance.Information provided by DuPont Performance Polymers
Tensile Stress 35.9 MPa

@Strain 9.20 %,
Temperature 40.0 °C
5210 psi

@Strain 9.20 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612  (Unverified Data**)