Polymer Property : Tensile Stress = 5280 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 36.4 MPa

@Strain 4.17 %,
Temperature 0.000 °C
5280 psi

@Strain 4.17 %,
Temperature 32.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC4601 NC010 Nylon  (Unverified Data**)
Plasticized Toughened Renewably Sourced Polyamide Developed for Extrusion Zytel RS LC4601 NC010 is a flexible toughened and plasticized polyamide resin intended for extrusion applications.Informatio..
Tensile Stress 36.4 MPa

@Temperature -40.0 °C
5280 psi

@Temperature -40.0 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET  (Unverified Data**)
Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio..