Mechanical Properties Metric English Comments
Tensile Stress 3.65 MPa

@Strain 100 %,
Temperature 23.0 °C
529 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7980-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7980-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Tensile Stress 3.65 MPa

@Strain 100 %,
Temperature 23.0 °C
529 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7980-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7980-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
Tensile Stress 3.65 MPa

@Strain 200 %
529 psi

@Strain 200 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ EG-9077 Thermoplastic Elastomer (TPE)
The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compoun..
Tensile Stress 3.65 MPa

@Strain 100 %,
Temperature 23.0 °C
529 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7980-1 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7980-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Tensile Stress 3.65 MPa

@Strain 100 %,
Temperature 23.0 °C
529 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7980-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylene - Rubbery Feel - Soft T..
Tensile Stress 3.65 MPa

@Strain 300 %,
Temperature 23.0 °C
529 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynalloy™ OBC 8100-N65 Thermoplastic Elastomer (TPE)
Dynalloy™ OBC8100-N65 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t..
Tensile Stress 3.65 MPa

@Strain 103.81 %,
Temperature 100 °C
529 psi

@Strain 103.81 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 3.65 MPa

@Strain 7.23 %,
Temperature 120 °C
529 psi

@Strain 7.23 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 3.65 MPa

@Strain 0.170 %,
Temperature 0.000 °C
529 psi

@Strain 0.170 %,
Temperature 32.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610  (Unverified Data**)
Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie..
Tensile Stress 3.65 MPa

@Strain 6.00 %,
Temperature 0.000 °C
529 psi

@Strain 6.00 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)