Mechanical Properties Metric English Comments
Tensile Stress 53.7 MPa

@Strain 6.60 %,
Temperature 0.000 °C
7790 psi

@Strain 6.60 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500AF Acetal (POM)  (Unverified Data**)
20% Teflon® Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AF is a medium viscosity acetal homopolymer resin containing 20% Teflon PTFE fibers. It is desi..
Tensile Stress 53.7 MPa

@Strain 4.70 %,
Temperature 40.0 °C
7790 psi

@Strain 4.70 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper..
Tensile Stress 53.7 MPa

@Strain 4.70 %,
Temperature 40.0 °C
7790 psi

@Strain 4.70 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration ..
Tensile Stress 53.7 MPa

@Strain 5.80 %,
Temperature 40.0 °C
7790 psi

@Strain 5.80 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and ..