Mechanical Properties Metric English Comments
Tensile Stress 55.63 MPa

@Strain 2.00 %,
Temperature 120 °C
8068 psi

@Strain 2.00 %,
Temperature 248 °F
ISO 527
DuPont Performance Polymers Crastin® SK608 BK509 PBT  (Unverified Data**)
Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 55.63 MPa

@Strain 4.13 %,
Temperature -40.0 °C
8068 psi

@Strain 4.13 %,
Temperature -40.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC4601 NC010 Nylon  (Unverified Data**)
Plasticized Toughened Renewably Sourced Polyamide Developed for Extrusion Zytel RS LC4601 NC010 is a flexible toughened and plasticized polyamide resin intended for extrusion applications.Informatio..