Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 55.63 MPa @Strain 2.00 %, Temperature 120 °C |
8068 psi @Strain 2.00 %, Temperature 248 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK608 BK509 PBT
(Unverified Data**) Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 55.63 MPa @Strain 4.13 %, Temperature -40.0 °C |
8068 psi @Strain 4.13 %, Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC4601 NC010 Nylon
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide Developed for Extrusion Zytel RS LC4601 NC010 is a flexible toughened and plasticized polyamide resin intended for extrusion applications.Informatio.. |