Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 56.53 MPa @Strain 8.18 %, Temperature 180 °C |
8199 psi @Strain 8.18 %, Temperature 356 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G35HSLR BK031 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G35HSLR BK031 is a 35% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i.. |