Mechanical Properties Metric English Comments
Tensile Stress 3.93 MPa

@Strain 300 %
570 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® N8960T TPE, Nylon Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInformation from Alliance Polymers & Se..
Tensile Stress 3.93 MPa

@Strain 200 %
570 psi

@Strain 200 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ EG-9082 Thermoplastic Elastomer (TPE)
The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compoun..
Tensile Stress 3.93 MPa

@Strain 300 %
570 psi

@Strain 300 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ XL-2055 Thermoplastic Polyolefin Elastomer (TPO (POE))
PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o..
Tensile Stress 3.93 MPa

@Strain 16.63 %,
Temperature 40.0 °C
570 psi

@Strain 16.63 %,
Temperature 104 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 3.93 MPa

@Strain 0.0400 %,
Temperature -20.0 °C
570 psi

@Strain 0.0400 %,
Temperature -4.00 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon  (Unverified Data**)
Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood..
Tensile Stress 3.93 MPa

@Strain 170.49 %,
Temperature 120 °C
570 psi

@Strain 170.49 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..
Tensile Stress 3.93 MPa

@Strain 23.01 %,
Temperature 120 °C
570 psi

@Strain 23.01 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET  (Unverified Data**)
44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin..
Tensile Stress 3.93 MPa

@Strain 0.500 %,
Temperature 150 °C
570 psi

@Strain 0.500 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 11C40 NC010 Nylon 66  (Unverified Data**)
40% Mineral Reinforced Polyamide 66 Minlon 11C40 NC010 is a 40% mineral reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers